PARTIAL DENTURE CASTING & SURGICAL ALLOYS
Cobalt, Chrome, High Heat casting Alloy
| Main Contents: Co~64% - Cr~30% - Mo~5% - Mn~0.6% |
BETAFLEX 3™, NP, HARD, T-80BF3
BETAFLEX Hard and Regular Cylinders. With excellent mechanical characteristics and castability. For completion of extreme precision framework.
Casting Temp. | Burnout Temp. | Melting- | Interval | T.C.E. | Brinell Hardness | Specific Gravity | Yield Strength | Elongation |
2700F° 1480C° | 1850F° 1010C° | 2500- 1370- | 2600F° 1425C° | 14.7 | 325 | 8.9 | 123,000 | 6% |
BETAFEX 4™, NP, Regular, T-80BF4
Main Contents: Co~64% - Cr~27% - Mo~6% - Mn~0.6%
Casting Temp. | Burnout Temp. | Melting- | Interval | T.C.E. | Brinell Hardness | Specific Gravity | Yield Strength | Elongation |
2650F° 1455C° | 1850F° 1010C° | 2475- 1357- | 2550F° 1400C° | 14.7 | 300 | 8.9 | 112,000 | 8% |
Suitable for the production of dental implant.
High luster, wearability and adjustability. With very good memory quality to maintain its sure fit. With additional hardness for extremely delicate framework. Exhibits properties over any international standards. Ideal combination of hardness and strength. No special casting technique is required. Will not tarnish in the mouth.